082140460910 prajaguna@gmail.com

Absorption of Fine Aggregate Test

ASTM C-128 AASHTO T-84   For determining the water absorption of fine aggregate at saturated surface dry.
Cone
Brass, 40 mm i.d at the top, 90 mm i.d at the bottom, 75 mm height.
Tamper
Machine steel,   340 gr   weight, 25 mm dia.
Mixing Bowl
Stainless steel, round type 24 cm diameter approx.
Glass Plate
10 cm thick, 30 x 30 cm
Volumetric Flask
Heat resistance glass 500 ml capacity
Spatula
Wooden handle, stainless steel blade, 10 cm length.